13th International Conference on Fracture June 16–21, 2013, Beijing, China -7- (a) 0.009 ms (b) 0.035 ms (c) 0.3 ms (d) 1.0 ms Figure 5. SPH simulation of projectile impact on MDF, left: coloured by von Mises stress (0 - 20 MPa), and right: coloured by plastic strain (0 - 0.006)