ICF13A

13th International Conference on Fracture June 16–21, 2013, Beijing, China -8- 5. Conclusions - Fracture toughness of different asphalt mixtures was determined experimentally using several SCB specimens at low temperature conditions. - The influence of asphalt characteristic specifications such as void percentage, aggregate type, aggregate size and binder type were studied on the value of mode I fracture toughness. - It was observed that the risk of low temperature fracturing in the asphalt mixtures increases for mixtures containing siliceous aggregates, smaller aggregate sizes, greater percentages of voids and higher penetration grades of the binders. References [1] A. Braham, W. Buttlar, F. Ni, Laboratory Mixed-Mode Cracking of Asphalt Concrete Using the Single-Edge Notch Beam, Road Mater Pave Des, 11, ( 2010) 947-968. [2] M. P. Wagoner, W. G. Buttlar, G. H. Paulino, Development of a Single-Edge Notched Beam Test for Asphalt Concrete Mixtures, Journal of Testing and Evaluation, 33, (2005), Paper ID JTE12579 [3] M. P. Wagoner, W. G. Buttlar, G. H. Paulino, P. Blankenship, Investigation of the Fracture Resistance of Hot-Mix Asphalt Concrete Using a Disk-Shaped Compact Tension Test, Transp Res Rec,1929, ( 2005)183-192. [4] H. Kim, M. P. Wagoner, W. G. Buttlar, Numerical fracture analysis on the specimen size dependency of asphalt concrete using a cohesive softening model, Constr Build Mater, 23, ( 2009) 2112-2120. [5] B. Behnia, E. V. Dave, S. Ahmed, W. G. Buttlar, H. Reis, Effects of Recycled Asphalt Pavement Amounts on Low-Temperature Cracking Performance of Asphalt Mixtures Using Acoustic Emissions, Transp Res Rec, 2208, (2011) 64-71. [6] M. Ameri, A. Mansourian, S. Pirmohammad, M.R.M Aliha, M.R. Ayatollahi, Mixed mode fracture resistance of asphalt concrete mixtures, Engng Fract Mech 93, (2012), 153-167. [7] J. H. Liu, Fatigue Life Evaluation of Asphalt Rubber Mixtures Using Semi-Circular Bending Test, Adv Mater Res, 255,(2011) , 3444-3449. [8] X. J. Li, M.O. Marasteanu, Using Semi Circular Bending Test to Evaluate Low Temperature Fracture Resistance for Asphalt Concrete, Exp Mech, 50,(2010) 867–876. [9] L. N. Mohammad, M. Kim, M. Elseifi, Characterization of Asphalt Mixture’s Fracture Resistance Using the Semi-Circular Bending (SCB) Test, 7th RILEM International Conference on Cracking in Pavements, RILEM Bookseries 4, (2012) 1-10. [10] A. A. A. Molenaar, A. Scarpas, X. Liu, G. Erkens, Semi-circular bending test; simple but useful. J Assoc Asphalt Tech, 71, (2002) 794–815.

RkJQdWJsaXNoZXIy MjM0NDE=