13th International Conference on Fracture June 16–21, 2013, Beijing, China 6. Appendix I – Tables TABLE 1 The Cathodic Current Density (mA/cm2) for Uninhibited Chemical Cleaning Solution Ic,u and Inhibited Solution Ic,I and the Inhibition Efficiency I% under Isothermal Conditions. (Inhibitor Concentration 60 PPM) Temperature (K) 303 313 323 RPM Ic,u Ic,I I% Ic,u Ic,I I% Ic,u Ic,I I% 0 15 1.6 89 39 5.5 86 57 8.8 85 600 4.6 0.5 89 14 1.6 88.6 36 3.3 90.8 1000 4.6 0.46 90 14 1.6 88.6 34 3.0 91 1400 4.8 0.51 89.4 15 1.7 88.7 34 3.5 89.7 TABLE 2 The Cathodic Current Density (mA/cm2) for Uninhibited Chemical Cleaning Solution under 60 kW/m2 Heat Transfer Rate. (The Interfacial Temperatures are Bracketed). Bulk Temperature (K) RPM 303 313 323 600 8 (322.7) 19 (330.5) 40 (339.9) 1000 7.3 (315.9) 17 (324.3) 39 (333.7) 1400 6.5 (312.3) 16 (321.6) 37 (331.4)