13th International Conference on Fracture June 16–21, 2013, Beijing, China -7- [3] E.S. Puchi, M.H. Staia, H. Hintermann, A. Pertuz, J. Chitty, Influence of Ni-P electroless coating on the fatigue behavior of plain carbon steels, Thin Solid Films, 290–291 (1996), 370–375. [4] J.A.M. Ferreria, J.D.M Costa, V. Lapa, Fatigue behaviour of 42Cr Mo4 steel with PVD coatings, Int. J. Fatigue, 19 (1997) 293–299. [5] J.A. Berrios, D.G. Teer, E.S. Puchi-Cabrera, Fatigue properties of a 316L stainless steel coated with different TiNx deposits, Surf. Coat. Technol., 148 (2001), 179–190. [6] D. Yonekura, H. Fukuda and R. Murakami, Influence of Deposition Bias Voltage on Fatigue Cracking Behavior of Chromium Nitride Film Deposited on Steel, Key Engineering Materials 353–358 (2007) 275–278. [7] G.H. Majzoobi, A.R. Ahmadkhani, The effects of multiple re-shot peening on fretting fatigue behavior of Al7075-T6, Surf. Coat. Technol., 205 (2010), 102–109. [8] S. Hotta, Y. Itou, K. Saruki, T. Arai, Fatigue strength at a number of cycles of thin hard coated steels with quench-hardenrd substrate. Surf. Coat. Technol., 73 (1995), 5–13. [9] P. Schlund, P. Kindermann, R. Schulte, H.G. Sockel, U. Schleinkofer, K. Gorting, W. Heinrich, Mechanical behaviour of PVD/CVD-coated hard metals under cyclic loads, Int. J. Refract. Met. Hard Mater., 17 (1999) 179–185. [10]T. Bell, Y. Sun1, A. Suhadi, Environmental and technical aspects of plasma nitrocarburising, Vacuum, 59 (2000) 14–23. [11] M. Berg, C.V. Budtz-Jørgensen, H. Reitz, K.O. Schweitz, J. Chevallier, P. Kringhøj, J. Bøttiger, On plasma nitriding of steels, Surf. Coat. Technol., 124 (2000) 25–31. [12]M. Keddam, Characterization of the nitrided layers of XC38 carbon steel obtained by R.F. plasma nitriding, Appl. Surf. Sci. 254 (2008) 2276–2280. [13]T. BELL and N.L. LOH, The Fatigue Characteristics of Plasma Nitrided Three Pct Cr-Mo Steel, J. Heat Treating, 2 (1982) 232–237. [14]Sule Yildiz Sirin, Kahraman Sirin, Erdinc Kaluc, Effect of the ion nitriding surface hardening process on fatigue behavior of AISI 4340 steel, Mater. Charact. 59 (2008) 351–358. [15]X.J. Cao, F. Yang, R. Murakami, in: Auckland (New Zealand), International Conference on Structural Integrity and Failure, vol. 7, 2010. [16]B. Golgeli, K. Genel, Fatigue strength improvement of a hard chromium plated AISI 4140 steel using a plasma nitriding pre-treatment, Fatigue Fract. Eng. Mater. Struct., 29 (2006) 105–111. [17]N. Yan, R. Murakami, Insup Lee, Fatigue Behavior of Plasma Radical Nitrided SCM435 Steel in Super-Long Life Regime, Met. Mater. Int., 17 (2011) 577–581. [18]B. Wu, P. Wang, Y.-S. Pyoun, J. Zhang, R. Murakami, Effect of ultrasonic nanocrystal surface modification on the fatigue behaviors of plasma-nitrided S45C steel, Surf. Coat. Technol., 213 (2012) 271–277. [19] E. Menthe, K.-T. Rie, Further investigation of the structure and properties of austenitic stainless steel after plasma nitriding, Surf. Coat. Technol., 116–119 (1999) 199–204. [20] B. Larisch, U. Brusky, H.-J. Spies, Plasma nitriding of stainless steels at low temperatures , Surf. Coat. Technol., 116–119 (1999) 205–211. [21]G.P. Singh, J. Alphonsa, P.K. Barhai, P.A. Rayjada, P.M. Raole, S. Mukherjee, Effect of surface roughness on the properties of the layer formed on AISI 304 stainless steel after plasma nitriding, Surf. Coat. Technol., 200 (2006) 5807–5811. [22] F. Borgioli, A. Fossati, E. Galvanetto, T. Bacci, G. Pradelli, Glow discharge nitriding of AISI 316L austenitic stainless steel: Influence of treatment pressure, Surf. Coat. Technol., 200 (2006) 5505–5513. [23]J.W. Zhang,L.T. Lu, K. Shiozawa, W.N. Zhou, W.H. Zhang, Effect of nitrocarburizing and post-oxidation on fatigue behavior of 35CrMo alloy steel in very high cycle fatigue regime, Int. J. Fatigue 33 (2011) 880–886. [24]T. Sakai, M. Takeda, K. Shiozawa, Y. Ochi, M. Nakajima, T. Nakamura and N. Oguma,
RkJQdWJsaXNoZXIy MjM0NDE=