13th International Conference on Fracture June 16–21, 2013, Beijing, China -8- Figure 5. Contour plots of LMM results for type 1 weldment corresponding to εtot = 1% on the outer fiber of plate and t = 5 hours of dwell period Figure 6. Contour plots of LMM results for type 2 weldment corresponding to εtot = 1% on the outer fiber of plate and t = 5 hours of dwell period