ICF13A

13th International Conference on Fracture June 16–21, 2013, Beijing, China -7- Symposium Proc. ASTM STP 1131, H.A.Ernst et al., eds., Philadelphia, (1992) 284-296. [17] A.T. Yokobori, Jr., T. Yokobori, T. Kuriyama, T. Kako, Y. Kaji, “Characterization of high temperature creep crack growth rate in terms of independent parameters”, Proc. of the Int. Conf. on Creep, JSME, I Mech E, ASME., (1986) 135-140. [18] A.T. Yokobori, Jr., T. Yokobori, “New concept to crack growth at high temperature creep and creep-fatigue,” Advances in Fracture Research, Proc. ICF7, K. Salama et al., eds., Pergamon Press, 2, (1989) 1723-1735. [19] A.T. Yokobori, Jr., T. Uesugi, T. Yokobori, A. Fuji, M. Kitagawa, I. Yamaya, M. Tabuchi, and K. Yagi, “Estimation of creep crack growth rate in IN-100 based on the Q* parameter concept”, J. of Materials Science, 33 (1998) 1555-1562.