ICF13A

13th International Conference on Fracture June 16–21, 2013, Beijing, China -9- [4] P.B. Prangnell, F. Haddadi, Y.C. Chen, Ultrasonic spot welding aluminum to steel for automotive applications-microstructure and optimization. Mater Sci Technol, 27 (2011) 617−624. [5] X. Qi, G. Song, Interfacial structure of the joints between magnesium alloy and mild steel with nickel as interlayer by hybrid laser-TIG welding. Mater Des, 31 (2010) 605–609. [6] V.K. Patel, S.D. Bhole, D.L. Chen, Microstructure and mechanical properties of dissimilar welded Mg-Al joints by ultrasonic spot welding technique. Sci Technol Weld Join, 17 (2012) 202−206. [7] R. Jahn, R. Cooper, D. Wilkosz, The effect of anvil geometry and welding energy of microstructures in ultrasonic spot welds of AA6111-T4. Metall Mater Trans A, 38 (2007) 570−583. [8] E. Hetrick, R. Jahn, L. Reatherford, J. Skogsmo, S. Ward, D. Wilkosz, J. Devine, K. Graff, R. Gehrin, Ultrasonic spot welding: A new tool for aluminum joining. Weld J, 84 (2005) 26−30. [9] P.B. Prangnell, D. Bakavos, Novel approaches to friction spot welding thin aluminium automotive sheet. Mater Sci Forum, 638-642 (2010) 1237−1242. [10] V.K. Patel, S.D. Bhole, D.L. Chen, Influence of ultrasonic spot welding on microstructure in a magnesium alloy. Scripta Mater, 65 (2011) 911–914. [11] S.H. Chowdhury, D.L. Chen, S.D. Bhole, X. Cao and P. Wanjara, Lap shear strength and fatigue life of friction stir spot welded AZ31 magnesium and 5754 aluminum alloys. Mater Sci Eng A, 556 (2012) 500–509 [12] D. Bakavos and P.B Prangnell, Mechanisms of joint and microstructure formation in high power ultrasonic spot welding 6111 aluminum automotive sheet. Mater Sci Eng A, 527 (2010) 6320−6334. [13] V.K. Patel, S.D. Bhole, D.L. Chen, Improving weld strength of magnesium to aluminum dissimilar joints via tin interlayer during ultrasonic spot welding. Sci Technol Weld Join, 17 (2012) 342–347. [14] D. Choi , B. Ahn ,C. Lee , Y. Yeon, K. Song, S. Jung, Formation of intermetallic compounds in Al and Mg alloy interface during friction stir spot welding. Intermetallics, 19 (2011) 125–130. [15] Y.C. Chen and K. Nakata, Friction stir lap joining aluminum and magnesium alloys. Scripta Mater, 58 (2008) 433–436. [16] Y.S. Sato, A. Shiota, H. Kokawa, K. Okamoto, Q. Yang, C. Kim, Effect of interfacial microstructure on lap shear strength of friction stir spot weld of aluminum alloy to magnesium alloy, Sci Tech Weld Join, 15 (2010) 319–324. [17] A. Panteli, Y. Chen, D. Strong, X. Zhang, P. Prangnell, Optimization of aluminum to magnesium ultrasonic spot welding. JOM, 64 (2012) 414–420. [18] L. Liu, X. Qi, Strengthening effect of nickel and copper interlayers on hybrid laser-TIG welded joints between magnesium alloy and mild steel. Mater Des, 31 (2010) 3960–3963. [19] M. Santella, T. Franklin, J. Pan, T.Y. Pan, E. Brown, Ultrasonic spot welding of AZ31B to galvanized mild steel. SAE Inter, 3 (2010) 652–657. [20] C. Schneider, T. Weinberger, J. Inoue, T. Koseki, N. Enzinger, Characterization of interface of steel/magnesium FSW. Sci Tech Weld Join, 16 (2011) 100–106. [21] S.H. Chowdhury, D.L. Chen, S.D. Bhole, X. Cao and P. Wanjara, Lap shear strength and fatigue behavior of friction stir spot welded dissimilar magnesium-to-aluminum joints with adhesive. Mater Sci Eng A, 562 (2013) 53–60. [22] W. Xu, D.L. Chen, L. Liu, H. Mori, Y. Zhou, Microstructure and mechanical properties of weld-bonded and resistance spot welded magnesium-to-steel dissimilar joints. Mater Sci Eng A, 537 (2012) 11–24. [23] L.M. Zhao, Z.D. Zhang, Effect of Zn interlayer on interface microstructure and strength of diffusion-bonded Mg-Al joints. Scripta Mater, 58 (2008) 283–286.

RkJQdWJsaXNoZXIy MjM0NDE=