ICF13A

Cover 1
The invariant integral: Some news - Genady P. Cherepanov 3
The characterization of dominating region of fracture (process region) around a crack tip based on the concept of mechanical similarity and atomic mechanics - Toshimitsu Yokobori, Yoshiko Nagumo, Takahiro Yajima, Toshihito Ohmi 12
Numerical and analytical prediction of GB microcrack initiation: Effect of material and microstructure parameters - Mohamed Ould Moussa, Maxime Sauzay, 21
Strain concentration in tensile, fatigue and fracture behaviour - Stephen D. Antolovich, Ronald W. Armstrong 31
The Cottrell Legacy: Metamorphosis of ICF into the World Academy of Structural Integrity 2011-2021 - Alberto Carpinteri, David M.R. Taplin 41
Sir Alan Cottrell and the dislocation mechanics of fracturing - Ronald W. Armstrong 45
A pipeline approach to developing virtual tests for composite materials - Brian Cox, Hrishikesh Bale, Matthew Blacklock 56
A Vibration Energy Harvester with Internal Impact and Hybrid Transduction Mechanisms - Songmao Chen 66
Effects of electric field and poling on the cyclic bending fatigue in cracked piezoceramics - Yasuhide Shindo, Fumio Narita, Masayuki Sato 76
Three-phase elliptical inclusions with an internal stress field of linear form - Xu Wang 85
Evaluation of strength recovery and analysis of damage progression of notched unidirectional carbon/epoxy composites encompassing selfhealing of interfacial debonding - Kazuaki Sanada, Yuta Mizuno, Yasuhide Shindo 95
Anti-plane moving polarization saturation crack in ferroelectric solids - Hao-Sen Chen, Dai-Ning Fang 101
Fracture criteria for piezoelectric ceramics - Leslie Banks-Sills 111
Experimental and analytical study of the effect of variable amplitude loadings in VHCF regime - Manuela Sander, Thomas Müller 118
Is there a threshold for PSB formation in iron - Chong Wang, Danièle Wagner, Qingyuan Wang, Claude Bathias 129
Subsurface non defect fatigue crack origin and local plasticity exhaustion - Guocai Chai 139
Application of Dang Van criterion to rolling contact fatigue in wind turbine roller bearings - Michele Cerullo 149
Effects of microstructure on very-high-cycle fatigue crack initiation and life scatter for a high strength steel - Zhengqiang Lei, Youshi Hong, Jijia Xie 159
Very high cycle fatigue for single phase ductile materials: Microplasticity and energy dissipation - Veronique Favier, Ngoc L. Phung, Nicolas Ranc 167
Evaluation of an ultrasonic device to test fretting-fatigue in very high cycle regime - Pedro Filgueiras, Claude Bathias, Ernani Palma 176
Gigacycle fatigue behaviors in Fusion Zone and Heat Affected Zone of Q345 LA steel welded joints - Liu Yongjie, Tian Renhui, He Chao 186
Very high cycle fatigue (VHCF) behavior of structured Al 2024 thin sheets - Sebastian Stille, Tilmann Beck, Lorenz Singheiser 196
Effect of yttrium content on the ultra-high cycle fatigue behavior of Mg-Zn-Y-Zr alloys - Daokui Xu, Enhou Han 204
Influence of high mean stresses on lifetime and damage of the martensitic steel X10CrNiMoV12-2-2 in the VHCF regime - Beck Tilmann, Stephan Kovacs, Lorenz Singheiser 211
Effect of aging condition on fatigue strength of maraging steel in long life region - Qiang Chen, Qingyuan Wang, Norio Kawagoishi 221
Influence of deformation-induced alpha prime martensite on the crack initiation mechanism in a metastable austenitic steel in the HCF and VHCF regime - Martina Zimmermann, Andrei Grigorescu, Carsten Mueller-Bollenhagen 229
Very high cycle fatigue strength of a high strength steel under sea water corrosion - Palin-Luc Thierry, Claude Bathias 238
3. Experimental results and discussion 240
Study of fatigue crack mechanism on an armco iron in the gigacycle fatigue by temperature recording and microstructural observations - Danièle Wagner, Chong Wang, Qingyuan Wang 248
Defect induced scaling in gigacycle fatigue - Vladimir Oborin, Mickail Bannikov, Oleg Naimark 257
The effect of damage accumulation in slip bands on the resonant behavior in the very high cycle fatigue (VHCF) regime - Philipp Hilgendorff, Andrei Grigorescu, Martina Zimmermann 263
Very high cycle fatigue behabvior of plasma nitrided 316 stainless steel - Daisuke Yonekura, Kei Ozaki, Ryota Shibahara 272
Experimental investigation on effects of various factors on very high cycle fatigue property for spring steels - Taku Miura, Tatsuo Sakai, Takayuki Sakakibara 280
Surface crack initiation pehenomenon in very high cycle fatigue - Muhammad Kashif Khan, Qingyuan Wang 290
Finite element modeling of the coupling between thermal dissipation and fish-eye crack growth in very high cycle fatigue regime - Laurent Gallimard, Quan H. Nguyen, Claude Bathias 300
Investigations of subcritical crack propagation under high cycle fatigue - Attilio Arcari, Nagaraja Iyyer, Kittur Madan 306
The significance of two-phase plasticity for the crack initiation process during very high cycle fatigue of duplex steel - Alexander Giertler, Marcus Söker, Benjamin Dönges 317
Microplasticity, microdamage, microcracking in ultrasonic fatigue - C. Bathias, D. Field, S. Antolovich, P.C. Paris 325
An interaction integral method for 2D elastodynamic crack problems - Zhiyong Wang, Li Ma, Linzhi Wu 335
The eXtended Finited Element Method for frictional contact problem - Zhiqiang Hu, Guogang Fan, Gao Lin 342
Implementation of the extended finite element method for hydraulic fracture problems - Zuorong Chen 352
Thermal shock residual strength of ultra-high temperature ceramics with the consideration of temperature - Dingyu Li, Weiguo Li, Ruzhuan Wang 362
UHPC precast product under severe freeze-thaw conditions - Ming-Gin Lee, Kun-Long Lee, Mang Tia 370
Novel direct method on the life prediction of component under high temperature—creep fatigue conditions - Haofeng Chen 378
Creep crack initiation and growth behavior in weldments of high Cr steels - Ryuji Sugiura, Toshimitsu Yokobori, Kazuto Sato 388
Three-dimensional vacancy diffusion analysis related to micro damage of C(T) specimen for P92 steel under creep condition - Haruhisa Shigeyama, A. Toshimitsu Yokobori Jr., Ryuji Sugiura 395
Evaluation of creep damage and fracture in high Cr steel welds - Masaaki Tabuchi 404
Fracture based testing and modelling, and component fracture based testing and modelling, and component life assessment of welds - Kamran Nikbin 411
Integrity increasing of damaged steel pipelines using external and internal reinforcing - Janos Lukacs, Gyula Nagy, Imre Torok 423
Based on cycle strain damage prediction of the crack growth behavior of elliptic surface crack - Long Chen, Lixun Cai, Kaikai Shi 433
Effect of pitch difference on anti-loosening performance for high strength bolts and nuts - Xin Chen, Yu-Ichiro Akaishi, Nao-Aki Noda 443
Research on the new low temperature self-protective pasty boronizing processes of thermal power plant economizer pipe - Jianjun He, Jian Chen, Yan Ren 453
LCF behavior and life modeling of DZ125 under complicated load condition at high temperature - Jia Huang, Xiaoguang Yang, Duoqi Shi 459
Effect of SiC partilces on fatigue crack propagation of spray-formed SiC particulate-reinforced Al–Si alloy composites - Wei Li, Jian Chen, Jianjun He 472
Interlaminar shear strength for three kinds of ceramic matrix composites at 1173K - Jianjie Gou, Chengyu Zhang, Shengru Qiao 482
Atomistic simulation of fatigue crack growth in α-Fe under high temperature - Tong Liu, Minshan Liu 490
Comparing crack growth testing and simulation results under thermo-mechanical fatigue conditions - Ramesh Chandwani, Christopher M. Timbrell, Steve Jacques 501
Reliability of micro/macro-fatigue crack growth behavior in the wires of cable-stayed bridge - Keke Tang 511
Development of classical boundary element analysis of fracture mechanics in gradient materials - Quentin Z.Q. Yue Quentin Z.Q. Yue, Hong Tian Xiao 521
A BEM for transient coupled thermoelastic crack analysis of homogeneous/functionally graded bimaterials - Chuanzeng Zhang, Alexander Ekhlakov, Oksana Khay 530
Crack growth-based fatigue life prediction using spline fictitious boundary element method - Cheng Su, Chun Zheng 540
Null-field integral approach for the piezoelectricity problems with arbitrary elliptical inhomogeneities - Ying-Te Lee, Jeng-Tzong Chen, Shyh-Rong Kuo 549
Modeling the effect of residual stress on the ductile fracture behavior of an aluminum alloy 5083-H116 - Xiaosheng Gao, Jun Zhou 559
Mechanisms for cleavage fracture in duplex stainless steels- Guocai Chai, Peter Stenvall 569
Cleavage modelling with experimental particle size distribution and novel particle failure criterion - Andrey P Jivkov, Peter James 579
Load history effects on fracture toughness of RPV steel - Jérémy Hure, Benoît Tanguy 589
Fracture Toughness Predictions Using the Weibull Stress Model with Implications for Estimations of the T0 Reference Temperature - Claudio Ruggieri, Rafael Savioli, Robert H. Dodds Jr. 599
A Local Approach to Creep-Fatigue -Oxidation Interactions in Inco 718 Alloy - André Pineau, Raul De Moura Pinho, Stéphane Pierret 609
On Modeling of Thermal Embrittlement in PWR Steels using the Local Approach to Fracture - Antoine Andrieu, André Pineau, Pierre Joly 620
Hierarchical Damage Simulation to Correlate Micro-structural Characteristics of Steel with Ductile Crack Growth Resistance of Component - Mitsuru Ohata, Hiroto Shoji, Fumiyoshi Minami 630
Integrated Damage Mechanics Approach to Brittle and Ductile Crack Propagation - Geralf Hütter, Thomas Linse, Uwe Mühlich 640
1. Introduction 640
2. Model 641
3. Results 644
Acknowledgement 647
References 647
Application of damage models to the ductile-brittle transition region of Reactor steels - Thomas Linse, Meinhard Kuna 648
Application of the Local Approach for Prediction of Ductile Fracture of Highly Irradiated Austenitic Steels - Boris Margolin, Alexander Sorokin, Victor Kostylev 658
Stress-Controlled and Stress-and-Strain Controlled Criteria of Brittle Fracture in Local Approach - Victoria Shvetsova, Boris Margolin, Alexander Gulenko 669
Scatter of measured KIC related to the scatters of local parameters Xf, σf and εpc - Jian Hong Chen, Rui Cao 679
The Elusive Temperature Dependence of the Master Curve - Kim Wallin 687
Local Approach Applied to the Fracture Toughness of Resistance Spot Welds - Florent Krajcarz, Anne-Françoise Gourgues-Lorenzon, Emmanuel Lucas 696
Analysis of a singular stress field near the edge of joint using molecular dynamics - Hideo Koguchi, Nobuyasu Suzuki 706
Chirality and Size Dependent Elastic Properties of Silicene Nanoribbons under Uniaxial Tension - Yuhang Jing, Yi Sun, Hongwei Niu 717
Dislocation dynamics analysis of hydrogen embrittlement in alpha iron based on atomistic investigations - Shinya Taketomi, Honami Imanishi, Ryosuke Matsumoto 723
Finite Element Simulation of Crack Propagation for α-Ti Based on Cohesive Zone Law Deriving from Molecular Dynamics - Yi Liao, Xiangguo Zeng, Jun Chen 732
Finite Element Simulation of Interfacial Fracture between Fe3C and α-Fe Based on Cohesive Zone Law Deriving from Molecular Dynamics - Taolong Xu, Xiangguo Zeng, Anlin Yao 742
Tunable Negative Poisson’s Ratio of 3D Spanned-Fullerene Nanotube Nanotruss - Jianyang Wu, Jianying He, Zhiliang Zhang 753
Influence of Interfacial Mechanical Properties on Elongation of Multilayered Composite Metals - Tomotsugu Shimokawa 761
Failure mode transition of Zr-based bulk metallic glass - Fan Zeng, LanHong Dai 767
On bifurcation of homogenous deformation in metallic glasses - Yan Chen, Lanhong Dai 773
Mesh Dependence of Transverse Cracking in Laminated Stainless Steel with both High Strength and High Ductility - Xian Guo, Wenjun Zhang, Jian Lu 782
Hamiltonian analysis applied to the dynamic crack growth and arrest in a Double Cantilever Beam - Gilles DEBRUYNE, Radhi ABDELMOULA 787
The concepts and properties of nanoskin materials and components created by ultrasonic nanocrystal surface modification - Young Shik Pyoun, Qingyuan Wang, Muhammad Kashif Khan 797
Efficient simulation of crack growth in multiple-crack systems considering internal boundaries and interfaces - Paul Judt, Andreas Ricoeur 805
Crack Growth Life Assessment on Turbine Component under Combined Fatigue Loading - Dianyin Hu, Rongiqao Wang, Huawei Liu 815
Numerical investigation of the fracture behavior of tungsten at the micro scale - Christopher Bohnert, Sabine M Weygand, Nicola J. Schmitt 824
Mechanics Mechanism of Re-fracturing in Inclusion Reservoirs - Xue Shifeng Xue Shifeng, Chen Xinmin, Han Zhongying 833
On propagation of interface cracks parallel to free boundaries in relation to delamination of multilayered coatings - Konstantin B. Ustinov, Robert Goldstein 840
On the Formation of Regular Crack Networks around a Circular Hole under Uniform Compression - Ilya Nickolaevich Dashevskiy 849
Fatigue Crack Growth Modelling in Welded Stiffened Panels under Cyclic Tension - Željko Božić, Siegfried Schmauder, Marijo Mlikota 859
Numerical study of the fracture behavior of an electron beam welded steel joint by cohesive zone modeling - Haoyun Tu, Siegfried Schmauder, Ulrich Weber 869
Solidification Cracking of IN 718 TIG Welds - Myriam Brochu, Alexis Chiocca, Rafael Navalon-Cabanes 878
Mechanical properties of lattice truss structures made of a selective laser melted superalloy - Håkan Brodin, Jonas Saarimäki 888
Evaluation of Optimal Condition in Laser Shock Peening Process by AE Method - Tomoki Takata, Manabu Enoki, Akinori Matsui 898
Low Frequency Laser Ultrasonics for Evaluation of Internal Cracks in Multi-layered Steels - Sho Ikeda, Kaita Ito, Shoichi Nambu 908
Mode I Fatigue Crack Growth Behaviour in a Welded Cruciform Joint under Biaxial Stresses - Xiang Zhang, Haiying Zhang, Rui Bao 909
Ultrasonic Spot Welding of Lightweight Alloys - V.K. Patel, S.D. Bhole, D.L. Chen 919
Analysis and residual strength prediction for multiple site damage in aircraft structures by using weight function method - X.R. Wu, W. Xu, H. Wang 929
Effect of welding defects on plastic behaviour and fatigue lifetime of friction stir welded Al-Cu-Li alloy - Thomas Le Jolu, Thilo F. Morgeneyer, Anne Denquin 939
Fibre Bridging and Crack Tip Shielding in Glare: Numerical and Experimental Validation - Sunil Bhat 949
Short/Small Crack Model Development for Aircraft Structural Life Assessment - Min Liao, Guillaume Renaud, Yan Bombardier 959
Deformations and Damage Evolution of Austenitic Steel AISI304 with Martensite Phase Transformation - Gang Han, Huang Yuan 969
The local concept to assess weldment with help of nano-indentation and FEM simulation - Jie Fang, Huang Yuan 980
Application of Fluid-Solid Couple on Multidisciplinary Optimization Design for Turbine Blade - JIA Zhi-gang, WANG Rong-qiao, HU Dian-yin 989
Application of Fluid-Solid Couple on Multidisciplinary Optimization Design for Turbine Blade 989
JIA Zhi-gang1,*, WANG Rong-qiao2, HU Dian-yin2, FAN Jiang2, Shen Xiu-li2 989
1 China aviation engine establishment, Beijing, 100028, China 989
Abstract The multi-field coupled analysis, a higher precision, is an interaction effect among the fluid, the structure strength and the thermal on the turbine design. Considering the coupled effect in the multidisciplinary optimization design (MDO) c... 989
Keywords fluid-solid closely coupled analysis; multidisciplinary design optimization (MDO); variable complexity method (VCM); collaborative optimization (CO) strategy; turbine design; 989
1. Introduction 989
2. Turbine Fluid-Solid Coupled Analysis 990
2.1. ALE Problem of Fluid-Solid Couple 990
2.2. Dynamic Grid Technology and Coupled Step Settings 990
2.3. Process of Fluid-Solid Coupled Analysis Based on ALE 991
3. MDO technologies 991
3.1. Various precise models 991
3.2. Periodic Updating Method 992
3.3. Two-Point Scale Function 992
3.4. Multiple-Precision Optimization Strategy 993
4. Coupled Analysis and MDO on the turbine blade 994
4.1. Model Parameters 994
4.2. Result Analysis of Coupled Calculation on Turbine Blade 995
4.3. Optimization Model of Turbine Blade Based on CO Strategy 996
4.4. Optimization Results Analysis 997
Conclusion 999
References 1000
Influence of high temperature ageing on the toughness of advanced heat resistant materials - Mattias Calmunger, Guocai Chai, Sten Johansson 1001
Experimental Studies of Thermal Aging Effects on the Tensile and Tearing Fracture Behavior of Carbon Black Filled Rubbers - Xiaoling Hu, Yan Li, Xiu Liu 1009
A fracture-based model of periodic-arrayed indentation for rock cutting - Yu Jun Xie, Bo Yang Xiang, Xiao Zhi Hu 1014
Theoretical Analysis of Effects of Confining Pressure on the Stress Intensity Factors for Cracked Brazilian Disk - Jigang Xu, Shiming Dong, Zhenlin Wang 1023
Separation of the Energy Release Rate of Fracture - Tianmin Guo 1032
Fracture Analysis of Particulate MEE Materials Using a Domain-Independent Interaction Integral Method - Hongjun Yu, Linzhi Wu 1044
Buckling Analysis of a Nanowire Lying on Winkler-Pasternak Elastic Foundation - Tiankai Zhao, Jun Luo 1054
Effect of thermally activated energy on dislocation emission from a blunted crack tip - X. Zeng, Q.H. Fang, Y.W. Liu 1059
Effect of cooperative grain boundary sliding and migration on emission of dislocations from a crack tip in nanocrystalline materials - H. Feng, Q.H. Fang, Y.W. Liu 1068
Flat-tipped Indentation Fracture Mechanics - Xiaozhi Hu, Yujun Xie 1080
Free edge coupling effect of piezoelectric cross-ply laminated plates - Chao Han Chao Han, Zhangjian Wu 1089
Improvement of crack-tip stress series with Padé approximants - Gaëtan Hello, Mabrouk Ben-Tahar, Jean-Marc Roelandt 1099
On Symmetric Crack Formation in Plates under Central Bending - Ilya Nickolaevich Dashevskiy 1108
Edge dislocation emission from nanovoid with the effect of neighboring nanovoids and surface stress - Yingxin Zhao, Qihong Fang, Youwen Liu 1116
Edge dislocation emission from nanovoid with the effect of neighboring nanovoids and surface stress - Yingxin Zhao, Qihong Fang, Youwen Liu 1125
Multi-scale modeling and diffraction-based characterization of elastic behaviour of human enamel - Tan Sui, Michael A. Sandholzer, Nikolaos Baimpas 1134
Fracture toughness measurements on bovine enamel by indentation techniques - J. Rodríguez, M.A. Garrido, L. Ceballos 1144
Study of the Mechanical Properties of Bones Under Fracture Healing Conditions with Specific Medical Treatments, Using 4 Point Bending Tests and Ultra-Micro Indentation Techniques - Soraya Diego, Estela Ruiz, José A. Casado 1153
Determination of the mechanical properties of normal and calcified human mitral chordae tendineae - José A. Casado, Soraya Diego, Diego Ferreño 1163
Understanding Backspatter due to Skull Fracture from a Ballistic Projectile - Raj Das, Justin Fernandez, Alistair Collins 1173
All-Atom CSAW: An Ab Initio Protein Folding Method - Weitao Sun 1183
Technology in Locomotion and Domotic Control for Quadriplegic - Mauricio Plaza, Oscar Avilés, William Aperador 1189
The Crack Growth Behavior in electrolyte membrane under Mechanical-electrochemical Loading - Yun J Chen, Yi Sun, Yi Z Liu 1198
Mechanisms of failure in porcelain-veneered sintered zirconia restorations - Tan Sui, Kalin Dragnevski, Tee K. Neo 1206
Cracking simulation of ceramic materials under thermal shock by a non-local fracture model - Li Jia, Song Fan, Jiang Chiping 1215
Mechanical Characterization of Sisal Fiber Reinforced Cement Mortar - Roberto Fujiyama, Fathi Darwish, Marcos Pereira 1225
Analysis of stress singularity field near the cross point of inclusion and free surface by 3D element free Galerkin method - Yasuyuki Tsukada, Takahiko Kurahashi, Hideo Koguchi 1232
Finite element analysis of erosive wear for offshore structure - Z.G. Liu, S. Wan, V.B. Nguyen 1239
Computational Method for Crack Layer Model - Haiying Zhang Haiying Zhang, Alexander Chudnovsky 1247
Modelling Damage in Nuclear Graphite - Thorsten Becker, James Marrow 1257
A Stabilized Sequential Coupling Algorithm for Hydro-mechanical Systems using Reproducing Kernel Particle Method - Yongning XIE, Gang WANG 1266
Random elasto-plastic lattice modeling of damage in fibrous materials - Keqiang Hu, Zengtao Chen, K. C. Li 1276
Cohesive Zone Analysis of Crack Propagation on a Hierarchical Structured Interface - Xiaoru Wang, Akihiro Nakatani 1286
Modeling of cracked structures containing voids subjected to fatigue and dynamic loads using XFEM - Mohamed Riad KIRED, Brahim Elkhalil HACHI, Mohamed GUESMI 1296
Mixed mode computation of the dynamic stress intensity factor for cracked 2D structures with inclusion using XFEM - Alaa Eddine HOUA, Brahim Elkhalil HACHI, Mohamed GUESMI 1301
Size Effect Analysis of Recycled Concrete Fracture based on Micromechanics Using the Base Force Element Method - Yijiang Peng, Nana Dang, Lijuan Zhang 1306
Identification of fracture process under moisture variation in wood materials - Frédéric Dubois, Rostand Moutou Pitti, Eric Fournely 1316
T-stress evaluation in nonhomogeneous materials under thermal loading by means of interaction energy integral method - Fengnan Guo, Licheng Guo, Hongjun Yu 1326
Torsional properties of bamboo-like structured Cu nanowires - Haifei Zhan, Yuantong Gu 1332
Computational prediction of fracture toughness of polycrystalline metals - Yan Li, David L. McDowell, Min Zhou 1341
Residual stress effects on the propagation of fatigue cracks in the weld of a CA6NM stainless steel - Alexandre Trudel, Myriam Brochu, Martin Lévesque 1349
Cutting zone temperature and specific cutting energy measurements and evaluation in machining metals - Y. Yifrach, U. Ben-Hanan 1359
Modeling of Damage Evolution in Particulate Reinforced Composites with VCFEM - Ran Guo, Wenyan Zhang, Benning Qu 1369
A New Interface Element for Shell Structures Delamination Analysis - Biao Li, Yazhi Li, Jie Su 1377
Advanced remeshing techniques for complex 3D crack propagation - Vincent Chiaruttini, Vincent Riolo, Frederic Feyel 1383
Time-Domain BEM for Dynamic Crack Problems in Thin Piezoelectric Structures - Hongjun Zhong, Jun Lei, Chuanzeng Zhang 1392
Transient Dynamic Crack Analysis in Decagonal Quasicrystal - Vladimir Sladek, Jan Sladek, Slavomir Krahulec 1401
Finite Deformation Modeling of Crystalline Defects in Hyper-elastic Material - Akihiro Nakatani, Mitsuhiro Akita 1411
Investigation on 3D fatigue crack propagation in surface-cracked specimens - X. Li, H. Yuan, J.Y. Sun 1418
Wedge Splitting Test on Fracture Behaviour of Fiber Reinforced and Regular High Performance Concretes - Kamil Hodicky, Thomas Hulin, Jacob W. Schmidt 1426
Instability and failure of particulate materials caused by rolling of non-spherical particles - Elena Pasternak, Arcady V. Dyskin 1436
Mechanism of in-plane fracture growth in particulate materials based on relative particle rotations - Arcady V. Dyskin, Elena Pasternak 1446
Simulation of Damage and Crack Propagation in Three-Point Bending Asphalt Concrete Beam - Guowei Zeng, Xinhua Yang, Fan Bai 1456
A New LEFM Based Description of Concrete Fracture and Size Effects - Kim Wallin 1465
Effect of Characteristic Specifications on Fracture Toughness of Asphalt Concrete Materials - Hamid Behbahani, MohammadReza. M. Aliha, Hassan Fazaeli 1475
A constitutive approach to fracture simulation based on augmented virtual internal bond method - Zhennan Zhang, Shaofeng Yao 1484
Investigation on the Failure Mechanisms in Sandstones under Uniaxial Compression by Digital Image Correlation - Ganyun Huang, Hao Zhang, Haipeng Song 1491
Rock fracture toughness testing using SCB specimen - M. R. Ayatollahi, M. J. Alborzi 1497
Modeling Fracture Processes in Numerical Concrete - Zhiwei Qian, Erik Schlangen, Guang Ye 1504
Stability and fracture analysis of arch dam based on deformation reinforcement theory - Yuanwei Pan, Yaoru Liu, Qiang Yang 1510
Acoustic emission detection in concrete specimens: experimental analysis and simulations by a lattice model - I. Iturrioz, G. Lacidogna, A. Carpinteri 1517
Particle simulation of AE statistics and fracture in concrete TPB test - Alberto Carpinteri, Giuseppe Lacidogna, Stefano Invernizzi 1531
Numerical Modeling on the Stress-Strain Response and Fracture of Modeled Recycled Aggregate Concrete - Wengui Li, Jianzhuang Xiao, David J. Corr 1540
Determination of Residual Fracture Toughness of Post-fire Concrete Using Analytical and Weight Function Method - Kequan YU, Zhoudao LU, jiangtao YU 1551
Initiation and Propagation Behavior of a Fatigue Crack of Maraging Steel in High Humidity - Qiang Chen, Takanori Nagano, Yuzo Nakamura 1563
Crystallographic texture helps reduce HIC cracking in pipeline steels - José M. Hallen, Victoria Venegas, Francisco Caleyo 1572
Stress Corrosion Cracking Behavior of Wrought Magnesium Alloy AZ31 and AZ61 under Controlled Cathodic Potentials - Toshifumi Kakiuchi, Yoshihiko Uematsu, Masaki Nakajima 1579
The influence of sea water corrosion on the resistance cracking performance of carbon steel - Wang Limin, Han Daoping, Zhang Donghuan 1587
Cohesive Zone Model for Intergranular Slow Crack Growth in Zirconia and Ceramic: Influence of the water concentration and Microstructure - Bassem El Zoghbi, Rafael Estevez, Christian Olagnon 1592
Performance Deregulation Rule of Aircraft Fatigue Critical Components in Consideration of Calendar Environment - Chao Gao, Yuting He, Haiwei Zhang 1602
Developing New Innovative Descaling and Corrosion Inhibiting Solutions to Protect Steel Equipment in the Oil and Gas Industry - Abdulghani A. Jaralla, Muhannad M. Al-Darbi 1610
Crack initiation: stress-corrosion crack in X-52 pipeline steel in near-neutral pH environment - Mimoun Elboujdaini, Bingyan Fang, Rrg Eadie 1619
Recent developments in brittle and quasi-brittle failure assessment of graphite by means of SED approach - Filippo Berto, Paolo Lazzarin, M.R. Ayatollahi 1632
Stress state dependent failure loci of a talc-filled polypropylene material under static loading and dynamic loading - Shaoting Lin, Yong Xia, Chin-Hsu Lin 1640
Molecular Dynamics Simulation of Fracture of Graphene - M. A. N. Dewapriya, R. K. N. D. Rajapakse, A. Srikantha Phani 1656
Experimental study of heat dissipation process into fatigue crack tip in titanium alloys. - M.V. Bannikov, A.I. Terekhina, A.Y. Fedorova 1662
CTOD fracture toughness assessment method of High-strength steel based on BS7910 - Ziyu Xia, Zhangmu Miao, Tao Ma 1670
Crack Nucleation in Phase Field Fracture Models - Charlotte Kuhn, Ralf Müller 1680
Design based on ductile-brittle transition temperature for API 5L X65 steel used for dense CO2 transport - G Pluvinage, J Capelle, Z Azari 1690
Fracture toughness criteria of small-size specimens with ultrafine-grained structure - Yevgeny Deryugin 1700
A coupled stress and energy model for mixed-mode cracking of adhesive joints - Philipp Weißgraeber, Wilfried Becker 1708
Plastic factor of front face compact tension specimens - KAIKAI SHI, LIXUN CAI, CHEN BAO 1716
Continuous vs. Discontinuous Crack Extension: Characterization of Ductile Tearing in Thin Plates - Volodymyr P. Naumenko 1723
Influence of the residual stresses on the crack deflection in ceramic laminates - Oldrich Sevecek, Michal Kotou, Tomas Profant 1733
Application of a novel finite element method to design of splices in a fiber metal subjected to coupled thermo-mechanical loading - XueCheng Ping, MengCheng Chen, BingBing Zheng 1743
Examination on a Criterion for a Debonding Fracture of Single Lap Joints from the Intensity of Singular Stress Field - Tatsujiro Miyazaki, Nao-Aki Noda, Rong Li 1753
Fatigue delamination growth of composite laminates with fiber bridging: Theory and simulation - Lei Peng, Jifeng Xu 1760
Microstructure and properties of welding joint of 8%Ni high strength steel - R. Cao, J. H. Chen, Y. Peng 1770
A fracture-mechanics-based non-local damage model for crack prediction in brittle materials - Zhang Xiao-Bing, Li Jia 1780
Ferritic-pearlitic ductile cast irons: is ΔK a useful parameter? - Francesco Iacoviello, Vittorio Di Cocco, Alessandra Rossi, Mauro Cavallini 1790
Modeling of Strain Localization and Failure in Vanadium under Quasistatic Loading - Anastasia Kostina, Yuriy Bayandin, Oleg Plekhov 1799
Electrification of Glass by Fracture - Li Xie, Dewen Sun, Jun Zhou 1809
Influence of Microstructure on Fatigue Crack Propagation and Fracture Toughness of Large Ti-6Al-4V Cast Structure - Xin Feng, Anqi Wang, Yingjie Ma 1816
A New Damage Identification Strategy for SHM based on FBGs and Bayesian Model Updating Method - Yanhui Zhang, Wenyu Yang 1823
Сriticality of Damage-Failure Transitions under Dynamic and Fatigue Loading - Oleg Naimark 1833
Dynamic fracture of metals in wide range of strain rates - Alexander E. Mayer 1843
An Equivalent Strain Gradient Theory for Evolvement of Damage in void Material - Hong Zuo, Fangwen Wang, Teng Hou 1852
Singular Thermo-Elastic Stress Analysis of An Irregular Shaped Inclusion - MengCheng Chen, XueCheng Pin 1862
A Mechanism-Based Approach for Predicting Ductile Fracture of Metallic Alloys - Xiaosheng Gao 1870
Effect of pre-existing microcrack on the cyclic displacement instability in thermal barrier coating systems - Luochuan Su, Weixu Zhang, T.J. Wang 1880