13th International Conference on Fracture June 16–21, 2013, Beijing, China -4- (a) Tensile strain maps in IF steel (b) Width strain maps in IF steel (c) Tensile strain maps in AA5754 (d) Width strain maps in AA5754 (e) Tensile strain maps in AZ31 (f) Width strain maps in AZ31 Fig. 3 Deformation development occurring during uniaxial tensile tests