13th International Conference on Fracture June 16–21, 2013, Beijing, China -7- [5] MENG Xiancheng, WANG Yong, LIU Yazhengm, Analysis of pencil-tip shaped fracture of cord steel 72A during cold drawing and improvement of process, Special steel, 30(2009) 55-57. [6] YAO Ganying, PAN Yingjun, Causes of brittle fracture of 82B wire rod, Journal of Wuhan University of Science and Technology(Natural Science Edition), 29(2006) 457-459. [7] CAO Wenkui, XU Zhongliang, FANG Feng, etc, Fracture analysis of high carbon steel strand welding zone, Jiangsu Merallury, 34(2006) 6-9. [8] MA Peng, OU Yangqi, FU Junhong, etc, Cause analysis of SWRH82B wire rod drawing fracture, Metal Products, 36(2010) 57-59